AWS D1.1:2025 · Tabel 5.11 · Kategori B

Preheat A36 untuk GMAW — up to 3/4"

Suhu pemanasan awal dan antar lajur minimum untuk A36 dilas dengan GMAW pada ketebalan up to 3/4", sesuai AWS D1.1:2025 Tabel 5.11.

Berdasarkan AWS D1.1:2025 Tabel 5.11 — setiap nilai dilacak ke pasal.

Suhu Minimum Pemanasan Awal dan Antar Lajur
32°F / 0°C
Kategori B
Proses SMAW, SAW, GMAW atau FCAW hidrogen rendah
AWS D1.1:2025 Tabel 5.11, §5.7
Bila suhu logam dasar di bawah 32°F [0°C], panaskan awal hingga minimum 70°F [20°C] dan pertahankan selama pengelasan (Tabel 5.11 catatan kaki a).
Alat referensi. Verifikasi terhadap edisi yang berlaku dan WPS yang disetujui Insinyur.

GMAW (Gas Metal Arc Welding)

GMAW (MIG) feeds continuous solid wire with shielding gas — an inherently low-hydrogen process assigned to Category B in Table 5.11.

ER70S-6 wire at 0.035" or 0.045" diameter handles most structural work on common grades. Spray transfer at 250-350 amps provides high deposition for shop fillet welds. For thinner material under 1/4", short-circuit transfer at lower parameters reduces heat input. Gas flow rates of 35-45 CFH through a standard nozzle provide adequate shielding in typical shop environments without excessive turbulence.

A36

ASTM A36 is the most commonly specified structural steel in North America, with a minimum yield strength of 36 ksi and 58-80 ksi tensile range. It appears in both Category A (non-low-hydrogen SMAW) and Category B (low-hydrogen processes) of Table 5.11. A36 is available as plate (up to 8" thick), W-shapes, channels, angles, and bars from virtually every domestic mill. Its moderate carbon content (0.26% max for shapes, 0.25% max for plate up to 3/4") and typical carbon equivalent of 0.35-0.42 give it good weldability across all prequalified processes. A36 plate thicker than 1-1/2" carries a slightly higher carbon limit of 0.29%, while plate from 3/4" to 1-1/2" stays at 0.25% max.

Mengapa Preheat Ini untuk A36 dengan GMAW

Widely used structural carbon steel with 36 ksi yield and 0.26% max carbon. With low-hydrogen GMAW, this combination falls under Category B rather than Category A, reflecting the lower hydrogen potential of the consumable. The 32°F minimum preheat is lower than what non-low-hydrogen SMAW would require at the same thickness. Low-hydrogen electrodes and inherently low-hydrogen wire processes reduce the driving force for hydrogen-induced cracking in the heat-affected zone.

Aplikasi Umum untuk A36

Common in angle-to-gusset fillet welds, beam web clip angles, stiffener plates, base plate bearing connections, light bracing members, stair stringers, handrail posts, and miscellaneous steel fabrication. A36 plate is the default choice for connection elements such as shear tabs, moment end plates under 36 ksi demand, and simple beam-to-column seated connections. In retrofit and renovation, A36 angles and channels are standard for reinforcement brackets and framing infill. Typical shop drawing callouts include 3/8" and 1/2" A36 plate for gussets, 5/16" fillet welds on clip angles, and partial joint penetration groove welds on base plate stiffeners. A36 is so ubiquitous that most structural steel shops maintain permanent inventory in multiple thicknesses from 1/4" through 2" plate. Fillet weld sizes on A36 connections typically range from 3/16" minimum to 5/8" for heavy gusset-to-column welds, with E70XX electrodes providing significant overmatching strength.

Mengapa Preheat Penting pada up to 3/4"

Thin material sheds heat quickly, allowing hydrogen to escape the HAZ readily — lowest preheat tier in Table 5.11.

Baja Lain dengan GMAW pada up to 3/4"

BajaKategoriPreheat
A53 Gr.BB32°F (0°C)
A633 Gr.EC50°F (10°C)
A709 HPS70WC50°F (10°C)
A710 Gr.AC50°F (10°C)

Coba Kombinasi Berbeda

Gunakan kalkulator preheat interaktif untuk mencari kombinasi baja, proses, dan ketebalan dari D1.1:2025 Tabel 5.11.

Berapa preheat minimum untuk A36 dengan GMAW pada up to 3/4"?
Untuk A36 dilas dengan GMAW pada ketebalan up to 3/4", suhu preheat minimum adalah 32°F (0°C) sesuai AWS D1.1:2025 Tabel 5.11, Kategori B.
Kategori Tabel 5.11 apa yang berlaku untuk A36 dengan GMAW?
A36 dilas dengan GMAW termasuk Kategori B di AWS D1.1:2025 Tabel 5.11. Proses SMAW, SAW, GMAW atau FCAW hidrogen rendah. Pada ketebalan up to 3/4", kategori ini memerlukan preheat minimum 32°F (0°C).
Apakah A36 memerlukan preheat pada up to 3/4"?
Pada ketebalan up to 3/4" dengan GMAW, preheat minimum adalah 32°F (0°C) — secara efektif suhu ambien di atas titik beku. Tidak diperlukan pemanasan awal aktif kecuali logam dasar di bawah 32°F.

Data referensi D1.1:2025. Tidak berafiliasi dengan AWS.