AWS D1.1:2025 · Tablo 5.11 · Kategori A

A500 Gr.B/C için SMAW (non-low-hydrogen) Ön Isıtma — up to 3/4"

AWS D1.1:2025 Tablo 5.11'e göre up to 3/4" kalınlıkta SMAW (non-low-hydrogen) ile kaynaklanan A500 Gr.B/C için minimum ön ısıtma ve pasolar arası sıcaklık.

AWS D1.1:2025 Tablo 5.11 tabanlı — her değer maddeye kadar izlenmiştir.

Minimum Ön Isıtma ve Pasolar Arası Sıcaklık
32°F / 0°C
Kategori A
Düşük hidrojen olmayan SMAW prosesi
AWS D1.1:2025 Tablo 5.11, §5.7
Ana metal sıcaklığı 32°F [0°C] altında olduğunda, minimum 70°F [20°C]'ye ön ısıtma yapın ve kaynak sırasında sürdürün (Tablo 5.11 dipnot a).
Referans aracı. Proje uygulanabilir sürüm ve Mühendis onaylı KPŞ ile doğrulayın.

SMAW (Non-Low-Hydrogen)

Non-low-hydrogen SMAW (E6010/E6011) uses cellulosic electrodes with higher hydrogen potential, assigned to Category A in Table 5.11.

For common structural shapes and plate, non-low-hydrogen SMAW with E6010 or E6011 excels at root passes on open-root groove welds where burn-through control matters. Vertical-up technique with a slight weave keeps the puddle manageable. Rod consumption runs about 10-12 electrodes per pound of weld metal deposited. Electrode stubs should be no shorter than 2 inches to maintain adequate arc length control.

A500 Gr.B/C

ASTM A500 Grade B (46 ksi yield for round, 42 ksi for rectangular) and Grade C (50 ksi round, 46 ksi rectangular) cover cold-formed welded and seamless structural tubing — round, square, and rectangular HSS sections. These are the standard tubular members in building frames, trusses, and signage structures, produced in wall thicknesses from 16 gauge (0.065") up to 5/8" for rectangular and 1/2" for round. Table 5.11 assigns both Category A and B preheat requirements. The cold-forming process work-hardens the corners, producing corner radii with higher hardness (up to 20% increase) and reduced ductility compared to the flat faces. This affects welding behavior at corner locations, particularly on heavily loaded connection details where weld starts or stops near corner radii can create initiation points for fatigue cracks.

SMAW ile A500 Gr.B/C için Bu Ön Isıtma Neden

Cold-formed structural tubing for HSS sections in frames and trusses. At this thickness, SMAW with non-low-hydrogen electrodes places the joint in Category A of Table 5.11. The minimum preheat of 32°F compensates for the higher diffusible hydrogen from cellulosic electrode coatings. The thicker the material, the longer hydrogen takes to escape the heat-affected zone, which is why preheat rises with thickness even for this common grade.

A500 Gr.B/C için Tipik Uygulamalar

Standard for HSS columns in office buildings, hollow section trusses in warehouse roofs, exposed architectural tube steel, sign structures, solar panel racking frames, greenhouse frames, and guard rail posts. A500 tube-to-tube moment connections require through-plate or diaphragm detailing to transfer forces across the closed section. Slotted gusset connections into HSS bracing members are a signature fabrication detail requiring careful fit-up and beveling of the gusset plate. Common sizes include HSS 6x6x3/8 and HSS 8x8x1/2 for columns, HSS 4x4x1/4 for bracing, and HSS 10x6x3/8 for rectangular beam applications. The cold-formed corner radius creates a heat-affected zone consideration that differs from hot-rolled shapes when planning multi-pass weld sequences. Round HSS pipe columns are also common, typically HSS 6.625x0.280 through HSS 12.750x0.500 for mezzanine posts and canopy supports. Fillet welds connecting HSS to cap plates and base plates are the most frequent weld joint detail.

up to 3/4"'de Ön Isıtma Neden Önemlidir

Thin material sheds heat quickly, allowing hydrogen to escape the HAZ readily — lowest preheat tier in Table 5.11.

A500 Gr.B/C için Neden 32°F?

Minimum 32°F (0°C) ön ısıtma, donma koşullarının üzerinde aktif ön ısıtma gerekmediği anlamına gelir. Bu kalınlıkta Tablo 5.11 Kategori A, A500 Gr.B/C'in düşük hidrojen olmayan SMAW ile yeterli sünekliğe ve düşük karbon eşdeğerine sahip olması nedeniyle ortam minimumunu atar. Dipnot (a)'ya göre, 32°F altında çalışırken bağlantıyı en az 70°F (20°C)'ye ön ısıtın ve kaynak sırasında sürdürün.

up to 3/4"'de SMAW (non-low-hydrogen) ile Diğer Çelikler

ÇelikKategoriÖn Isıtma
A36A32°F (0°C)
A53 Gr.BA32°F (0°C)

SMAW (non-low-hydrogen) ile A500 Gr.B/C

Farklı Kombinasyonları Dene

D1.1:2025 Tablo 5.11'den herhangi bir çelik, proses ve kalınlık kombinasyonunu aramak için interaktif ön ısıtma hesap makinesini kullanın.

up to 3/4"'de SMAW ile A500 Gr.B/C için minimum ön ısıtma nedir?
up to 3/4" kalınlıkta SMAW (non-low-hydrogen) ile kaynaklanan A500 Gr.B/C için minimum ön ısıtma sıcaklığı AWS D1.1:2025 Tablo 5.11, Kategori A'e göre 32°F (0°C)'dir.
SMAW ile A500 Gr.B/C için hangi kategori geçerlidir?
SMAW (non-low-hydrogen) ile kaynaklanan A500 Gr.B/C, AWS D1.1:2025 Tablo 5.11'de Kategori A altına girer. Düşük hidrojen olmayan SMAW prosesi. up to 3/4" kalınlıkta bu kategori minimum 32°F (0°C) ön ısıtma gerektirir.
up to 3/4"'de A500 Gr.B/C ön ısıtma gerektirir mi?
up to 3/4" kalınlıkta SMAW (non-low-hydrogen) ile minimum ön ısıtma 32°F (0°C)'dir — donma noktasının üzerinde etkin olarak ortam sıcaklığı. Ana metal 32°F altında olmadıkça aktif ön ısıtma gerekmez.

D1.1:2025 referans verileri. AWS ile bağlantılı değildir.