AWS D1.1:2025 · Tablo 5.11 · Kategori B

A36 için GMAW Ön Isıtma — over 2-1/2"

AWS D1.1:2025 Tablo 5.11'e göre over 2-1/2" kalınlıkta GMAW ile kaynaklanan A36 için minimum ön ısıtma ve pasolar arası sıcaklık.

AWS D1.1:2025 Tablo 5.11 tabanlı — her değer maddeye kadar izlenmiştir.

Minimum Ön Isıtma ve Pasolar Arası Sıcaklık
225°F / 110°C
Kategori B
Düşük hidrojen SMAW, SAW, GMAW veya FCAW prosesi
AWS D1.1:2025 Tablo 5.11, §5.7
Referans aracı. Proje uygulanabilir sürüm ve Mühendis onaylı KPŞ ile doğrulayın.

GMAW (Gas Metal Arc Welding)

GMAW (MIG) feeds continuous solid wire with shielding gas — an inherently low-hydrogen process assigned to Category B in Table 5.11.

ER70S-6 wire at 0.035" or 0.045" diameter handles most structural work on common grades. Spray transfer at 250-350 amps provides high deposition for shop fillet welds. For thinner material under 1/4", short-circuit transfer at lower parameters reduces heat input. Gas flow rates of 35-45 CFH through a standard nozzle provide adequate shielding in typical shop environments without excessive turbulence.

A36

ASTM A36 is the most commonly specified structural steel in North America, with a minimum yield strength of 36 ksi and 58-80 ksi tensile range. It appears in both Category A (non-low-hydrogen SMAW) and Category B (low-hydrogen processes) of Table 5.11. A36 is available as plate (up to 8" thick), W-shapes, channels, angles, and bars from virtually every domestic mill. Its moderate carbon content (0.26% max for shapes, 0.25% max for plate up to 3/4") and typical carbon equivalent of 0.35-0.42 give it good weldability across all prequalified processes. A36 plate thicker than 1-1/2" carries a slightly higher carbon limit of 0.29%, while plate from 3/4" to 1-1/2" stays at 0.25% max.

GMAW ile A36 için Bu Ön Isıtma Neden

Widely used structural carbon steel with 36 ksi yield and 0.26% max carbon. With low-hydrogen GMAW, this combination falls under Category B rather than Category A, reflecting the lower hydrogen potential of the consumable. The 225°F minimum preheat is lower than what non-low-hydrogen SMAW would require at the same thickness. Low-hydrogen electrodes and inherently low-hydrogen wire processes reduce the driving force for hydrogen-induced cracking in the heat-affected zone.

A36 için Tipik Uygulamalar

Common in angle-to-gusset fillet welds, beam web clip angles, stiffener plates, base plate bearing connections, light bracing members, stair stringers, handrail posts, and miscellaneous steel fabrication. A36 plate is the default choice for connection elements such as shear tabs, moment end plates under 36 ksi demand, and simple beam-to-column seated connections. In retrofit and renovation, A36 angles and channels are standard for reinforcement brackets and framing infill. Typical shop drawing callouts include 3/8" and 1/2" A36 plate for gussets, 5/16" fillet welds on clip angles, and partial joint penetration groove welds on base plate stiffeners. A36 is so ubiquitous that most structural steel shops maintain permanent inventory in multiple thicknesses from 1/4" through 2" plate. Fillet weld sizes on A36 connections typically range from 3/16" minimum to 5/8" for heavy gusset-to-column welds, with E70XX electrodes providing significant overmatching strength.

over 2-1/2"'de Ön Isıtma Neden Önemlidir

The heaviest sections demand the highest preheat in Table 5.11. Multi-pass sequences require maintaining interpass temperature throughout.

over 2-1/2"'de GMAW ile Diğer Çelikler

ÇelikKategoriÖn Isıtma
A53 Gr.BB225°F (110°C)
A633 Gr.EC300°F (150°C)
A709 HPS70WC300°F (150°C)
A710 Gr.AC300°F (150°C)

Farklı Kombinasyonları Dene

D1.1:2025 Tablo 5.11'den herhangi bir çelik, proses ve kalınlık kombinasyonunu aramak için interaktif ön ısıtma hesap makinesini kullanın.

over 2-1/2"'de GMAW ile A36 için minimum ön ısıtma nedir?
over 2-1/2" kalınlıkta GMAW ile kaynaklanan A36 için minimum ön ısıtma sıcaklığı AWS D1.1:2025 Tablo 5.11, Kategori B'e göre 225°F (110°C)'dir.
GMAW ile A36 için hangi kategori geçerlidir?
GMAW ile kaynaklanan A36, AWS D1.1:2025 Tablo 5.11'de Kategori B altına girer. Düşük hidrojen SMAW, SAW, GMAW veya FCAW prosesi. over 2-1/2" kalınlıkta bu kategori minimum 225°F (110°C) ön ısıtma gerektirir.
over 2-1/2"'de A36 için ön ısıtma neden 225°F?
over 2-1/2"'de GMAW ile A36 için 225°F ön ısıtma, çeliğin sertleşebilirliği ve bu kalınlıktaki artan kısıtlamanın kombinasyonunu yansıtır.

D1.1:2025 referans verileri. AWS ile bağlantılı değildir.