AWS D1.1:2025 · 표 5.11 · 범주 B

A572 Gr.50 GMAW 예열 — 3/4" to 1-1/2"

AWS D1.1:2025 표 5.11에 따른 A572 Gr.50의 GMAW 용접 시 3/4" to 1-1/2" 두께에서의 최소 예열 및 층간 온도.

AWS D1.1:2025 표 5.11 기반 — 모든 값이 조항까지 추적됨.

최소 예열 및 층간 온도
50°F / 10°C
범주 B 저수소 SMAW, SAW, GMAW 또는 FCAW 공정
AWS D1.1:2025 표 5.11, §5.7
참조 도구. 프로젝트 적용 판본 및 엔지니어 승인 WPS와 대조 확인하십시오.

Have a preheat question? Ask Flux

GMAW (Gas Metal Arc Welding)

GMAW (MIG) feeds continuous solid wire with shielding gas — an inherently low-hydrogen process assigned to Category B in Table 5.11.

ER70S-6 wire at 0.035" or 0.045" diameter handles most structural work on common grades. Spray transfer at 250-350 amps provides high deposition for shop fillet welds. For thinner material under 1/4", short-circuit transfer at lower parameters reduces heat input. Gas flow rates of 35-45 CFH through a standard nozzle provide adequate shielding in typical shop environments without excessive turbulence.

GMAW Tips for Common Structural Steels

For A572 Grade 50 structural steel (50 ksi yield, Category B only — non-LH SMAW is not prequalified), GMAW spray transfer with 0.045" ER70S-6 at 260–300 A is the standard shop process for W-shape connection plates, gusset plates, and base plates. Use 90/10 Ar/CO2 for improved bead profile on connection plate groove welds for moment frames.

Typical values for reference — always verify against your approved WPS and electrode manufacturer data.

Filler Metal for GMAW

Common wire: ER70S-6 (AWS A5.18). Diameter: 0.035" for thin sections and out-of-position, 0.045" for production flat/horizontal. Shielding gas: 75/25 Ar/CO2 (standard), 90/10 Ar/CO2 (less spatter, better profile), or 100% CO2 (deeper penetration, more spatter). Contact-tip-to-work distance: 1/2" to 3/4".

Typical values for reference — always verify against your approved WPS and electrode manufacturer data.

A572 Gr.50

ASTM A572 Grade 50 (50 ksi minimum yield, 65 ksi minimum tensile) is the dominant high-strength low-alloy structural steel in building construction. Most W-shapes rolled today are dual-certified A572/A992, with actual yield typically 50-58 ksi. It falls under Category B only in Table 5.11 — non-low-hydrogen SMAW is not prequalified for this grade. Chemistry limits include 0.23% max carbon (shapes) and columbium (niobium) or vanadium microalloying for grain refinement, producing a typical CE-IIW of 0.40-0.45. A572 Gr.50 plate is available in thicknesses up to 6" and is the default grade for connection plates, gussets, and base plates in building construction when loads exceed A36 capacity. The Gr.42, 55, 60, and 65 grades exist but Gr.50 accounts for over 90% of A572 production.

GMAW를 사용한 A572 Gr.50의 이 예열 이유

Dominant 50 ksi HSLA structural steel often dual-certified with A992. This steel is prequalified only with low-hydrogen processes under Table 5.11. With GMAW, the continuous solid wire and gas shielding in GMAW produce inherently low hydrogen levels, typically 2-4 mL/100g. The 50°F minimum preheat balances the steel’s strength level and carbon equivalent against the hydrogen control provided by GMAW. Non-low-hydrogen SMAW is not an option for this grade under D1.1 prequalified WPS.

A572 Gr.50의 일반적인 용도

Dominates building construction for W-shape column splices, beam-to-column moment connections, braced frame gusset plates, base plates over 36 ksi demand, crane runway girder webs, and mezzanine floor beams. A572 Gr.50 plate is the standard for connection elements in seismic designs per AISC 341. Complete joint penetration groove welds at beam flanges are the most critical weld detail in moment frames. The most common connection plate thicknesses are 3/4" and 1" for moment end plates and 1/2" to 5/8" for shear tabs. Demand-critical welds in seismic applications require notch-tough filler metals meeting AISC 341 Section A3.4b supplemental requirements with CVN testing at -20°F. Column splice CJP welds at every 2-3 story intervals are typically 2G or 3G field welds requiring portable preheat equipment. Base plate welds to foundation embed plates carry the full column load and require strict preheat compliance on thicker plates.

3/4" to 1-1/2"에서 예열이 중요한 이유

Preheat climbs at this range as thicker material slows heat dissipation, trapping hydrogen at crack-susceptible grain boundaries.

3/4" to 1-1/2"에서 GMAW를 사용하는 다른 강재

강재범주예열
A36B50°F (10°C)
A633 Gr.EC150°F (65°C)
A709 HPS70WC150°F (65°C)
A710 Gr.AC150°F (65°C)

다양한 조합 시도

인터랙티브 예열 계산기를 사용하여 D1.1:2025 표 5.11의 모든 강재, 공정, 두께 조합을 조회하세요.

3/4" to 1-1/2"에서 GMAW를 사용하여 A572 Gr.50의 최소 예열은 얼마입니까?
3/4" to 1-1/2" 두께에서 GMAW로 용접하는 A572 Gr.50의 최소 예열 온도는 AWS D1.1:2025 표 5.11, 범주 B에 따라 50°F (10°C)입니다. 이것은 또한 최소 층간 온도입니다.
GMAW를 사용하는 A572 Gr.50에 어떤 범주가 적용됩니까?
GMAW로 용접하는 A572 Gr.50은 AWS D1.1:2025 표 5.11의 범주 B에 해당합니다. 저수소 SMAW, SAW, GMAW 또는 FCAW 공정. 3/4" to 1-1/2" 두께에서 이 범주는 최소 50°F (10°C)의 예열을 요구합니다.