AWS D1.1:2025 · 표 5.11 · 범주 B

A36 GMAW 예열 — 1-1/2" to 2-1/2"

AWS D1.1:2025 표 5.11에 따른 A36의 GMAW 용접 시 1-1/2" to 2-1/2" 두께에서의 최소 예열 및 층간 온도.

AWS D1.1:2025 표 5.11 기반 — 모든 값이 조항까지 추적됨.

최소 예열 및 층간 온도
150°F / 65°C
범주 B
저수소 SMAW, SAW, GMAW 또는 FCAW 공정
AWS D1.1:2025 표 5.11, §5.7
참조 도구. 프로젝트 적용 판본 및 엔지니어 승인 WPS와 대조 확인하십시오.

GMAW (Gas Metal Arc Welding)

GMAW (MIG) feeds continuous solid wire with shielding gas — an inherently low-hydrogen process assigned to Category B in Table 5.11.

ER70S-6 wire at 0.035" or 0.045" diameter handles most structural work on common grades. Spray transfer at 250-350 amps provides high deposition for shop fillet welds. For thinner material under 1/4", short-circuit transfer at lower parameters reduces heat input. Gas flow rates of 35-45 CFH through a standard nozzle provide adequate shielding in typical shop environments without excessive turbulence.

A36

ASTM A36 is the most commonly specified structural steel in North America, with a minimum yield strength of 36 ksi and 58-80 ksi tensile range. It appears in both Category A (non-low-hydrogen SMAW) and Category B (low-hydrogen processes) of Table 5.11. A36 is available as plate (up to 8" thick), W-shapes, channels, angles, and bars from virtually every domestic mill. Its moderate carbon content (0.26% max for shapes, 0.25% max for plate up to 3/4") and typical carbon equivalent of 0.35-0.42 give it good weldability across all prequalified processes. A36 plate thicker than 1-1/2" carries a slightly higher carbon limit of 0.29%, while plate from 3/4" to 1-1/2" stays at 0.25% max.

GMAW를 사용한 A36의 이 예열 이유

Widely used structural carbon steel with 36 ksi yield and 0.26% max carbon. With low-hydrogen GMAW, this combination falls under Category B rather than Category A, reflecting the lower hydrogen potential of the consumable. The 150°F minimum preheat is lower than what non-low-hydrogen SMAW would require at the same thickness. Low-hydrogen electrodes and inherently low-hydrogen wire processes reduce the driving force for hydrogen-induced cracking in the heat-affected zone.

A36의 일반적인 용도

Common in angle-to-gusset fillet welds, beam web clip angles, stiffener plates, base plate bearing connections, light bracing members, stair stringers, handrail posts, and miscellaneous steel fabrication. A36 plate is the default choice for connection elements such as shear tabs, moment end plates under 36 ksi demand, and simple beam-to-column seated connections. In retrofit and renovation, A36 angles and channels are standard for reinforcement brackets and framing infill. Typical shop drawing callouts include 3/8" and 1/2" A36 plate for gussets, 5/16" fillet welds on clip angles, and partial joint penetration groove welds on base plate stiffeners. A36 is so ubiquitous that most structural steel shops maintain permanent inventory in multiple thicknesses from 1/4" through 2" plate. Fillet weld sizes on A36 connections typically range from 3/16" minimum to 5/8" for heavy gusset-to-column welds, with E70XX electrodes providing significant overmatching strength.

1-1/2" to 2-1/2"에서 예열이 중요한 이유

Heavy plate with significant restraint and thermal mass — preheat is critical to maintain slow cooling for hydrogen escape.

1-1/2" to 2-1/2"에서 GMAW를 사용하는 다른 강재

강재범주예열
A53 Gr.BB150°F (65°C)
A633 Gr.EC225°F (110°C)
A709 HPS70WC225°F (110°C)
A710 Gr.AC225°F (110°C)

다양한 조합 시도

인터랙티브 예열 계산기를 사용하여 D1.1:2025 표 5.11의 모든 강재, 공정, 두께 조합을 조회하세요.

1-1/2" to 2-1/2"에서 GMAW를 사용하여 A36의 최소 예열은 얼마입니까?
1-1/2" to 2-1/2" 두께에서 GMAW로 용접하는 A36의 최소 예열 온도는 AWS D1.1:2025 표 5.11, 범주 B에 따라 150°F (65°C)입니다. 이것은 또한 최소 층간 온도입니다.
GMAW를 사용하는 A36에 어떤 범주가 적용됩니까?
GMAW로 용접하는 A36은 AWS D1.1:2025 표 5.11의 범주 B에 해당합니다. 저수소 SMAW, SAW, GMAW 또는 FCAW 공정. 1-1/2" to 2-1/2" 두께에서 이 범주는 최소 150°F (65°C)의 예열을 요구합니다.
1-1/2" to 2-1/2"에서 A36의 예열이 150°F인 이유는?
1-1/2" to 2-1/2"에서 GMAW로 용접하는 A36의 150°F 예열은 강재의 경화성과 이 두께에서의 증가된 구속력의 조합을 반영합니다.

D1.1:2025 참조 데이터. AWS와 무관.