AWS D1.1:2025 · Tableau 5.11 · Catégorie B

Préchauffage de A572 Gr.50 pour SAW — over 2-1/2"

Température minimale de préchauffage et entre passes pour A572 Gr.50 soudé avec SAW à over 2-1/2" d'épaisseur, selon AWS D1.1:2025 Tableau 5.11.

Basé sur AWS D1.1:2025 Tableau 5.11 — chaque valeur tracée à l'article.

Température Minimale de Préchauffage et Entre Passes
225°F / 110°C
Catégorie B
Procédé SMAW, SAW, GMAW ou FCAW bas hydrogène
AWS D1.1:2025 Tableau 5.11, §5.7
Outil de référence. Vérifier contre l'édition applicable au projet et DMOS approuvé par l'Ingénieur.

SAW (Submerged Arc Welding)

SAW submerges the arc beneath granular flux for highest deposition rates, flat/horizontal only. Category B in Table 5.11.

SAW with F7A2-EM12K wire/flux delivers the highest deposition rates for flat-position fillet welds on building steel. Typical parameters: 500-700 amps, 28-32 volts, 18-30 IPM travel speed. Flux consumption runs approximately equal to wire consumption by weight. Unfused flux recovery and recycling systems are standard in production shops to control consumable costs.

SAW Tips for Common Structural Steels

For A572 Grade 50 structural steel (50 ksi yield, Category B only), SAW F7A2-EM12K at 550–700 A is the dominant process for crane runway girder web-to-flange fillet welds, built-up column seams, and plate girder fabrication in building construction. The deep-penetrating SAW arc on A572 Gr.50 plate achieves excellent root fusion on fillet welds without back-gouging.

Typical values for reference — always verify against your approved WPS and electrode manufacturer data.

Filler Metal for SAW

Wire: EM12K or EL12 with matching flux (AWS A5.17). Common combo: F7A2-EM12K. Diameter: 3/32" or 7/64". Flux type: active (A) for single-pass, neutral (N) for multi-pass. Voltage: 28-34V. Current: 400-800A depending on joint size. Travel: 12-24 ipm.

Typical values for reference — always verify against your approved WPS and electrode manufacturer data.

A572 Gr.50

ASTM A572 Grade 50 (50 ksi minimum yield, 65 ksi minimum tensile) is the dominant high-strength low-alloy structural steel in building construction. Most W-shapes rolled today are dual-certified A572/A992, with actual yield typically 50-58 ksi. It falls under Category B only in Table 5.11 — non-low-hydrogen SMAW is not prequalified for this grade. Chemistry limits include 0.23% max carbon (shapes) and columbium (niobium) or vanadium microalloying for grain refinement, producing a typical CE-IIW of 0.40-0.45. A572 Gr.50 plate is available in thicknesses up to 6" and is the default grade for connection plates, gussets, and base plates in building construction when loads exceed A36 capacity. The Gr.42, 55, 60, and 65 grades exist but Gr.50 accounts for over 90% of A572 production.

Pourquoi ce Préchauffage pour A572 Gr.50 avec SAW

Dominant 50 ksi HSLA structural steel often dual-certified with A992. This steel is prequalified only with low-hydrogen processes under Table 5.11. With SAW, the submerged arc process with granular flux produces controlled hydrogen levels, with flux condition being the primary variable. The 225°F minimum preheat balances the steel’s strength level and carbon equivalent against the hydrogen control provided by SAW. Non-low-hydrogen SMAW is not an option for this grade under D1.1 prequalified WPS.

Applications Typiques de A572 Gr.50

Dominates building construction for W-shape column splices, beam-to-column moment connections, braced frame gusset plates, base plates over 36 ksi demand, crane runway girder webs, and mezzanine floor beams. A572 Gr.50 plate is the standard for connection elements in seismic designs per AISC 341. Complete joint penetration groove welds at beam flanges are the most critical weld detail in moment frames. The most common connection plate thicknesses are 3/4" and 1" for moment end plates and 1/2" to 5/8" for shear tabs. Demand-critical welds in seismic applications require notch-tough filler metals meeting AISC 341 Section A3.4b supplemental requirements with CVN testing at -20°F. Column splice CJP welds at every 2-3 story intervals are typically 2G or 3G field welds requiring portable preheat equipment. Base plate welds to foundation embed plates carry the full column load and require strict preheat compliance on thicker plates.

Pourquoi le Préchauffage est Important à over 2-1/2"

The heaviest sections demand the highest preheat in Table 5.11. Multi-pass sequences require maintaining interpass temperature throughout.

Autres Aciers avec SAW à over 2-1/2"

AcierCatégoriePréchauffage
A36B225°F (110°C)
A633 Gr.EC300°F (150°C)
A709 HPS70WC300°F (150°C)
A710 Gr.AC300°F (150°C)

Essayez Différentes Combinaisons

Utilisez le calculateur interactif de préchauffage pour consulter toute combinaison acier, procédé et épaisseur du D1.1:2025 Tableau 5.11.

Quel est le préchauffage minimum pour A572 Gr.50 avec SAW à over 2-1/2" ?
Pour A572 Gr.50 soudé avec SAW à over 2-1/2" d'épaisseur, la température minimale de préchauffage est 225°F (110°C) selon AWS D1.1:2025 Tableau 5.11, Catégorie B. C'est aussi la température minimale entre passes.
Quelle catégorie du Tableau 5.11 s'applique à A572 Gr.50 avec SAW ?
A572 Gr.50 soudé avec SAW relève de la Catégorie B dans AWS D1.1:2025 Tableau 5.11. Procédé SMAW, SAW, GMAW ou FCAW bas hydrogène. À over 2-1/2" d'épaisseur, cette catégorie exige un préchauffage minimum de 225°F (110°C).
Pourquoi le préchauffage est-il de 225°F pour A572 Gr.50 à over 2-1/2" ?
Le préchauffage de 225°F pour A572 Gr.50 à over 2-1/2" avec SAW reflète la combinaison de la trempabilité de l'acier et la contrainte accrue à cette épaisseur.

Données de référence D1.1:2025. Non affilié à l'AWS.