AWS D1.1:2025 · Tableau 5.11 · Catégorie B

Préchauffage de A36 pour GMAW — up to 3/4"

Température minimale de préchauffage et entre passes pour A36 soudé avec GMAW à up to 3/4" d'épaisseur, selon AWS D1.1:2025 Tableau 5.11.

Basé sur AWS D1.1:2025 Tableau 5.11 — chaque valeur tracée à l'article.

Température Minimale de Préchauffage et Entre Passes
32°F / 0°C
Catégorie B
Procédé SMAW, SAW, GMAW ou FCAW bas hydrogène
AWS D1.1:2025 Tableau 5.11, §5.7
Lorsque la température du métal de base est inférieure à 32°F [0°C], préchauffer à minimum 70°F [20°C] et maintenir pendant le soudage (Tableau 5.11 note a).
Outil de référence. Vérifier contre l'édition applicable au projet et DMOS approuvé par l'Ingénieur.

GMAW (Gas Metal Arc Welding)

GMAW (MIG) feeds continuous solid wire with shielding gas — an inherently low-hydrogen process assigned to Category B in Table 5.11.

ER70S-6 wire at 0.035" or 0.045" diameter handles most structural work on common grades. Spray transfer at 250-350 amps provides high deposition for shop fillet welds. For thinner material under 1/4", short-circuit transfer at lower parameters reduces heat input. Gas flow rates of 35-45 CFH through a standard nozzle provide adequate shielding in typical shop environments without excessive turbulence.

A36

ASTM A36 is the most commonly specified structural steel in North America, with a minimum yield strength of 36 ksi and 58-80 ksi tensile range. It appears in both Category A (non-low-hydrogen SMAW) and Category B (low-hydrogen processes) of Table 5.11. A36 is available as plate (up to 8" thick), W-shapes, channels, angles, and bars from virtually every domestic mill. Its moderate carbon content (0.26% max for shapes, 0.25% max for plate up to 3/4") and typical carbon equivalent of 0.35-0.42 give it good weldability across all prequalified processes. A36 plate thicker than 1-1/2" carries a slightly higher carbon limit of 0.29%, while plate from 3/4" to 1-1/2" stays at 0.25% max.

Pourquoi ce Préchauffage pour A36 avec GMAW

Widely used structural carbon steel with 36 ksi yield and 0.26% max carbon. With low-hydrogen GMAW, this combination falls under Category B rather than Category A, reflecting the lower hydrogen potential of the consumable. The 32°F minimum preheat is lower than what non-low-hydrogen SMAW would require at the same thickness. Low-hydrogen electrodes and inherently low-hydrogen wire processes reduce the driving force for hydrogen-induced cracking in the heat-affected zone.

Applications Typiques de A36

Common in angle-to-gusset fillet welds, beam web clip angles, stiffener plates, base plate bearing connections, light bracing members, stair stringers, handrail posts, and miscellaneous steel fabrication. A36 plate is the default choice for connection elements such as shear tabs, moment end plates under 36 ksi demand, and simple beam-to-column seated connections. In retrofit and renovation, A36 angles and channels are standard for reinforcement brackets and framing infill. Typical shop drawing callouts include 3/8" and 1/2" A36 plate for gussets, 5/16" fillet welds on clip angles, and partial joint penetration groove welds on base plate stiffeners. A36 is so ubiquitous that most structural steel shops maintain permanent inventory in multiple thicknesses from 1/4" through 2" plate. Fillet weld sizes on A36 connections typically range from 3/16" minimum to 5/8" for heavy gusset-to-column welds, with E70XX electrodes providing significant overmatching strength.

Pourquoi le Préchauffage est Important à up to 3/4"

Thin material sheds heat quickly, allowing hydrogen to escape the HAZ readily — lowest preheat tier in Table 5.11.

Autres Aciers avec GMAW à up to 3/4"

AcierCatégoriePréchauffage
A53 Gr.BB32°F (0°C)
A633 Gr.EC50°F (10°C)
A709 HPS70WC50°F (10°C)
A710 Gr.AC50°F (10°C)

Essayez Différentes Combinaisons

Utilisez le calculateur interactif de préchauffage pour consulter toute combinaison acier, procédé et épaisseur du D1.1:2025 Tableau 5.11.

Quel est le préchauffage minimum pour A36 avec GMAW à up to 3/4" ?
Pour A36 soudé avec GMAW à up to 3/4" d'épaisseur, la température minimale de préchauffage est 32°F (0°C) selon AWS D1.1:2025 Tableau 5.11, Catégorie B. C'est aussi la température minimale entre passes.
Quelle catégorie du Tableau 5.11 s'applique à A36 avec GMAW ?
A36 soudé avec GMAW relève de la Catégorie B dans AWS D1.1:2025 Tableau 5.11. Procédé SMAW, SAW, GMAW ou FCAW bas hydrogène. À up to 3/4" d'épaisseur, cette catégorie exige un préchauffage minimum de 32°F (0°C).
A36 nécessite-t-il un préchauffage à up to 3/4" ?
À up to 3/4" d'épaisseur avec GMAW, le préchauffage minimum est 32°F (0°C) — effectivement la température ambiante au-dessus du point de congélation. Aucun préchauffage actif n'est requis sauf si le métal de base est en dessous de 32°F.

Données de référence D1.1:2025. Non affilié à l'AWS.