AWS D1.1:2025 · الجدول 5.11 · الفئة B

التسخين المسبق لـ A36 مع GMAW — over 2-1/2"

الحد الأدنى لدرجة حرارة التسخين المسبق وبين الممرات لـ A36 الملحوم بـ GMAW عند سماكة over 2-1/2"، وفقاً لـ AWS D1.1:2025 الجدول 5.11.

مبني على AWS D1.1:2025 الجدول 5.11 — كل قيمة متتبعة إلى البند.

الحد الأدنى لدرجة حرارة التسخين المسبق وبين الممرات
225°F / 110°C
الفئة B
عملية SMAW أو SAW أو GMAW أو FCAW منخفضة الهيدروجين
AWS D1.1:2025 الجدول 5.11، §5.7
أداة مرجعية. تحقق من الإصدار المطبق على المشروع وإجراء اللحام المعتمد من المهندس.

GMAW (Gas Metal Arc Welding)

GMAW (MIG) feeds continuous solid wire with shielding gas — an inherently low-hydrogen process assigned to Category B in Table 5.11.

ER70S-6 wire at 0.035" or 0.045" diameter handles most structural work on common grades. Spray transfer at 250-350 amps provides high deposition for shop fillet welds. For thinner material under 1/4", short-circuit transfer at lower parameters reduces heat input. Gas flow rates of 35-45 CFH through a standard nozzle provide adequate shielding in typical shop environments without excessive turbulence.

A36

ASTM A36 is the most commonly specified structural steel in North America, with a minimum yield strength of 36 ksi and 58-80 ksi tensile range. It appears in both Category A (non-low-hydrogen SMAW) and Category B (low-hydrogen processes) of Table 5.11. A36 is available as plate (up to 8" thick), W-shapes, channels, angles, and bars from virtually every domestic mill. Its moderate carbon content (0.26% max for shapes, 0.25% max for plate up to 3/4") and typical carbon equivalent of 0.35-0.42 give it good weldability across all prequalified processes. A36 plate thicker than 1-1/2" carries a slightly higher carbon limit of 0.29%, while plate from 3/4" to 1-1/2" stays at 0.25% max.

لماذا هذا التسخين المسبق لـ A36 مع GMAW

Widely used structural carbon steel with 36 ksi yield and 0.26% max carbon. With low-hydrogen GMAW, this combination falls under Category B rather than Category A, reflecting the lower hydrogen potential of the consumable. The 225°F minimum preheat is lower than what non-low-hydrogen SMAW would require at the same thickness. Low-hydrogen electrodes and inherently low-hydrogen wire processes reduce the driving force for hydrogen-induced cracking in the heat-affected zone.

التطبيقات النموذجية لـ A36

Common in angle-to-gusset fillet welds, beam web clip angles, stiffener plates, base plate bearing connections, light bracing members, stair stringers, handrail posts, and miscellaneous steel fabrication. A36 plate is the default choice for connection elements such as shear tabs, moment end plates under 36 ksi demand, and simple beam-to-column seated connections. In retrofit and renovation, A36 angles and channels are standard for reinforcement brackets and framing infill. Typical shop drawing callouts include 3/8" and 1/2" A36 plate for gussets, 5/16" fillet welds on clip angles, and partial joint penetration groove welds on base plate stiffeners. A36 is so ubiquitous that most structural steel shops maintain permanent inventory in multiple thicknesses from 1/4" through 2" plate. Fillet weld sizes on A36 connections typically range from 3/16" minimum to 5/8" for heavy gusset-to-column welds, with E70XX electrodes providing significant overmatching strength.

لماذا يهم التسخين المسبق عند over 2-1/2"

The heaviest sections demand the highest preheat in Table 5.11. Multi-pass sequences require maintaining interpass temperature throughout.

أنواع فولاذ أخرى مع GMAW عند over 2-1/2"

الفولاذالفئةالتسخين المسبق
A53 Gr.BB225°F (110°C)
A633 Gr.EC300°F (150°C)
A709 HPS70WC300°F (150°C)
A710 Gr.AC300°F (150°C)

جرّب تركيبات مختلفة

استخدم حاسبة التسخين المسبق التفاعلية للبحث عن أي تركيبة من الفولاذ والعملية والسماكة من D1.1:2025 الجدول 5.11.

ما هو الحد الأدنى للتسخين المسبق لـ A36 مع GMAW عند over 2-1/2"؟
لـ A36 الملحوم بـ GMAW عند سماكة over 2-1/2"، الحد الأدنى لدرجة حرارة التسخين المسبق هو 225°F (110°C) وفقاً لـ AWS D1.1:2025 الجدول 5.11، الفئة B. هذا أيضاً الحد الأدنى لدرجة حرارة بين الممرات.
ما الفئة التي تنطبق على A36 مع GMAW؟
A36 الملحوم بـ GMAW يقع تحت الفئة B في AWS D1.1:2025 الجدول 5.11. عملية SMAW أو SAW أو GMAW أو FCAW منخفضة الهيدروجين. عند سماكة over 2-1/2"، تتطلب هذه الفئة تسخيناً مسبقاً بحد أدنى 225°F (110°C).
لماذا التسخين المسبق 225°F لـ A36 عند over 2-1/2"؟
التسخين المسبق بمقدار 225°F لـ A36 عند over 2-1/2" مع GMAW يعكس مزيج قابلية التصلب للفولاذ والقيد المتزايد عند هذه السماكة.

بيانات مرجعية D1.1:2025. غير تابع لـ AWS.