A36 Preheat for GMAW — over 2-1/2"
Minimum preheat and interpass temperature for A36 welded with GMAW at over 2-1/2" thickness, per AWS D1.1:2025 Table 5.11.
Low-hydrogen SMAW, SAW, GMAW, or FCAW process
GMAW (Gas Metal Arc Welding)
GMAW (MIG) feeds continuous solid wire with shielding gas — an inherently low-hydrogen process assigned to Category B in Table 5.11.
ER70S-6 wire at 0.035" or 0.045" diameter handles most structural work on common grades. Spray transfer at 250-350 amps provides high deposition for shop fillet welds. For thinner material under 1/4", short-circuit transfer at lower parameters reduces heat input. Gas flow rates of 35-45 CFH through a standard nozzle provide adequate shielding in typical shop environments without excessive turbulence.
A36
ASTM A36 is the most commonly specified structural steel in North America, with a minimum yield strength of 36 ksi and 58-80 ksi tensile range. It appears in both Category A (non-low-hydrogen SMAW) and Category B (low-hydrogen processes) of Table 5.11. A36 is available as plate (up to 8" thick), W-shapes, channels, angles, and bars from virtually every domestic mill. Its moderate carbon content (0.26% max for shapes, 0.25% max for plate up to 3/4") and typical carbon equivalent of 0.35-0.42 give it good weldability across all prequalified processes. A36 plate thicker than 1-1/2" carries a slightly higher carbon limit of 0.29%, while plate from 3/4" to 1-1/2" stays at 0.25% max.
Why This Preheat for A36 with GMAW
Widely used structural carbon steel with 36 ksi yield and 0.26% max carbon. With low-hydrogen GMAW, this combination falls under Category B rather than Category A, reflecting the lower hydrogen potential of the consumable. The 225°F minimum preheat is lower than what non-low-hydrogen SMAW would require at the same thickness. Low-hydrogen electrodes and inherently low-hydrogen wire processes reduce the driving force for hydrogen-induced cracking in the heat-affected zone.
Typical Applications for A36
Common in angle-to-gusset fillet welds, beam web clip angles, stiffener plates, base plate bearing connections, light bracing members, stair stringers, handrail posts, and miscellaneous steel fabrication. A36 plate is the default choice for connection elements such as shear tabs, moment end plates under 36 ksi demand, and simple beam-to-column seated connections. In retrofit and renovation, A36 angles and channels are standard for reinforcement brackets and framing infill. Typical shop drawing callouts include 3/8" and 1/2" A36 plate for gussets, 5/16" fillet welds on clip angles, and partial joint penetration groove welds on base plate stiffeners. A36 is so ubiquitous that most structural steel shops maintain permanent inventory in multiple thicknesses from 1/4" through 2" plate. Fillet weld sizes on A36 connections typically range from 3/16" minimum to 5/8" for heavy gusset-to-column welds, with E70XX electrodes providing significant overmatching strength.
Why Preheat Matters at over 2-1/2"
The heaviest sections demand the highest preheat in Table 5.11. Multi-pass sequences require maintaining interpass temperature throughout.
Other Steels with GMAW at over 2-1/2"
| Steel | Category | Preheat |
|---|---|---|
| A53 Gr.B | B | 225°F (110°C) |
| A633 Gr.E | C | 300°F (150°C) |
| A709 HPS70W | C | 300°F (150°C) |
| A710 Gr.A | C | 300°F (150°C) |
A36 with GMAW
Try Different Combinations
Use the interactive preheat calculator to look up any steel, process, and thickness combination from D1.1:2025 Table 5.11.
A36 Welding Guides
D1.1:2025 reference data. Not affiliated with AWS.