AWS D1.1:2025 · 表5.11 · カテゴリーB

A572 Gr.50のGMAW用予熱 — 3/4" to 1-1/2"

A572 Gr.50をGMAWで板厚3/4" to 1-1/2"で溶接する場合の最低予熱およびパス間温度。AWS D1.1:2025 表5.11に基づく。

AWS D1.1:2025 表5.11に基づく — すべての値は条項に追跡可能。

最低予熱・パス間温度
50°F / 10°C
カテゴリーB 低水素SMAW、SAW、GMAW、またはFCAWプロセス
AWS D1.1:2025 表5.11、§5.7
参考ツール。プロジェクト適用版およびエンジニア承認済みWPSで確認すること。

Have a preheat question? Ask Flux

GMAW (Gas Metal Arc Welding)

GMAW (MIG) feeds continuous solid wire with shielding gas — an inherently low-hydrogen process assigned to Category B in Table 5.11.

ER70S-6 wire at 0.035" or 0.045" diameter handles most structural work on common grades. Spray transfer at 250-350 amps provides high deposition for shop fillet welds. For thinner material under 1/4", short-circuit transfer at lower parameters reduces heat input. Gas flow rates of 35-45 CFH through a standard nozzle provide adequate shielding in typical shop environments without excessive turbulence.

GMAW Tips for Common Structural Steels

For A572 Grade 50 structural steel (50 ksi yield, Category B only — non-LH SMAW is not prequalified), GMAW spray transfer with 0.045" ER70S-6 at 260–300 A is the standard shop process for W-shape connection plates, gusset plates, and base plates. Use 90/10 Ar/CO2 for improved bead profile on connection plate groove welds for moment frames.

Typical values for reference — always verify against your approved WPS and electrode manufacturer data.

Filler Metal for GMAW

Common wire: ER70S-6 (AWS A5.18). Diameter: 0.035" for thin sections and out-of-position, 0.045" for production flat/horizontal. Shielding gas: 75/25 Ar/CO2 (standard), 90/10 Ar/CO2 (less spatter, better profile), or 100% CO2 (deeper penetration, more spatter). Contact-tip-to-work distance: 1/2" to 3/4".

Typical values for reference — always verify against your approved WPS and electrode manufacturer data.

A572 Gr.50

ASTM A572 Grade 50 (50 ksi minimum yield, 65 ksi minimum tensile) is the dominant high-strength low-alloy structural steel in building construction. Most W-shapes rolled today are dual-certified A572/A992, with actual yield typically 50-58 ksi. It falls under Category B only in Table 5.11 — non-low-hydrogen SMAW is not prequalified for this grade. Chemistry limits include 0.23% max carbon (shapes) and columbium (niobium) or vanadium microalloying for grain refinement, producing a typical CE-IIW of 0.40-0.45. A572 Gr.50 plate is available in thicknesses up to 6" and is the default grade for connection plates, gussets, and base plates in building construction when loads exceed A36 capacity. The Gr.42, 55, 60, and 65 grades exist but Gr.50 accounts for over 90% of A572 production.

A572 Gr.50とGMAWでこの予熱が必要な理由

Dominant 50 ksi HSLA structural steel often dual-certified with A992. This steel is prequalified only with low-hydrogen processes under Table 5.11. With GMAW, the continuous solid wire and gas shielding in GMAW produce inherently low hydrogen levels, typically 2-4 mL/100g. The 50°F minimum preheat balances the steel’s strength level and carbon equivalent against the hydrogen control provided by GMAW. Non-low-hydrogen SMAW is not an option for this grade under D1.1 prequalified WPS.

A572 Gr.50の代表的な適用例

Dominates building construction for W-shape column splices, beam-to-column moment connections, braced frame gusset plates, base plates over 36 ksi demand, crane runway girder webs, and mezzanine floor beams. A572 Gr.50 plate is the standard for connection elements in seismic designs per AISC 341. Complete joint penetration groove welds at beam flanges are the most critical weld detail in moment frames. The most common connection plate thicknesses are 3/4" and 1" for moment end plates and 1/2" to 5/8" for shear tabs. Demand-critical welds in seismic applications require notch-tough filler metals meeting AISC 341 Section A3.4b supplemental requirements with CVN testing at -20°F. Column splice CJP welds at every 2-3 story intervals are typically 2G or 3G field welds requiring portable preheat equipment. Base plate welds to foundation embed plates carry the full column load and require strict preheat compliance on thicker plates.

3/4" to 1-1/2"で予熱が重要な理由

Preheat climbs at this range as thicker material slows heat dissipation, trapping hydrogen at crack-susceptible grain boundaries.

GMAWと3/4" to 1-1/2"における他の鋼材

鋼材カテゴリー予熱
A36B50°F (10°C)
A633 Gr.EC150°F (65°C)
A709 HPS70WC150°F (65°C)
A710 Gr.AC150°F (65°C)

別の組み合わせを試す

インタラクティブ予熱計算機を使用して、D1.1:2025 表5.11のあらゆる鋼材・プロセス・板厚の組み合わせを検索できます。

3/4" to 1-1/2"でGMAWを使用したA572 Gr.50の最小予熱温度は?
A572 Gr.50をGMAWで3/4" to 1-1/2"の板厚で溶接する場合、最低予熱温度はAWS D1.1:2025 表5.11、カテゴリーBに基づき50°F(10°C)です。これはパス間温度の最低値でもあり、パス間でも継手が50°F以下に冷却されてはなりません。
A572 Gr.50とGMAWに適用される表5.11のカテゴリーは?
GMAWで溶接されたA572 Gr.50は、AWS D1.1:2025 表5.11のカテゴリーBに該当します。低水素SMAW、SAW、GMAW、またはFCAWプロセス。3/4" to 1-1/2"板厚では、このカテゴリーは最低予熱50°F(10°C)を要求します。