AWS D1.1:2025 · 表5.11 · カテゴリーA

A36のSMAW (non-low-hydrogen)用予熱 — up to 3/4"

A36をSMAW (non-low-hydrogen)で板厚up to 3/4"で溶接する場合の最低予熱およびパス間温度。AWS D1.1:2025 表5.11に基づく。

AWS D1.1:2025 表5.11に基づく — すべての値は条項に追跡可能。

最低予熱・パス間温度
32°F / 0°C
カテゴリーA
非低水素SMAWプロセス
AWS D1.1:2025 表5.11、§5.7
母材温度が32°F [0°C]未満の場合は、最低70°F [20°C]まで予熱し、溶接中も維持すること(表5.11 脚注a)。
参考ツール。プロジェクト適用版およびエンジニア承認済みWPSで確認すること。

SMAW (Non-Low-Hydrogen)

Non-low-hydrogen SMAW (E6010/E6011) uses cellulosic electrodes with higher hydrogen potential, assigned to Category A in Table 5.11.

For common structural shapes and plate, non-low-hydrogen SMAW with E6010 or E6011 excels at root passes on open-root groove welds where burn-through control matters. Vertical-up technique with a slight weave keeps the puddle manageable. Rod consumption runs about 10-12 electrodes per pound of weld metal deposited. Electrode stubs should be no shorter than 2 inches to maintain adequate arc length control.

A36

ASTM A36 is the most commonly specified structural steel in North America, with a minimum yield strength of 36 ksi and 58-80 ksi tensile range. It appears in both Category A (non-low-hydrogen SMAW) and Category B (low-hydrogen processes) of Table 5.11. A36 is available as plate (up to 8" thick), W-shapes, channels, angles, and bars from virtually every domestic mill. Its moderate carbon content (0.26% max for shapes, 0.25% max for plate up to 3/4") and typical carbon equivalent of 0.35-0.42 give it good weldability across all prequalified processes. A36 plate thicker than 1-1/2" carries a slightly higher carbon limit of 0.29%, while plate from 3/4" to 1-1/2" stays at 0.25% max.

A36とSMAWでこの予熱が必要な理由

Widely used structural carbon steel with 36 ksi yield and 0.26% max carbon. At this thickness, SMAW with non-low-hydrogen electrodes places the joint in Category A of Table 5.11. The minimum preheat of 32°F compensates for the higher diffusible hydrogen from cellulosic electrode coatings. The thicker the material, the longer hydrogen takes to escape the heat-affected zone, which is why preheat rises with thickness even for this common grade.

A36の代表的な適用例

Common in angle-to-gusset fillet welds, beam web clip angles, stiffener plates, base plate bearing connections, light bracing members, stair stringers, handrail posts, and miscellaneous steel fabrication. A36 plate is the default choice for connection elements such as shear tabs, moment end plates under 36 ksi demand, and simple beam-to-column seated connections. In retrofit and renovation, A36 angles and channels are standard for reinforcement brackets and framing infill. Typical shop drawing callouts include 3/8" and 1/2" A36 plate for gussets, 5/16" fillet welds on clip angles, and partial joint penetration groove welds on base plate stiffeners. A36 is so ubiquitous that most structural steel shops maintain permanent inventory in multiple thicknesses from 1/4" through 2" plate. Fillet weld sizes on A36 connections typically range from 3/16" minimum to 5/8" for heavy gusset-to-column welds, with E70XX electrodes providing significant overmatching strength.

up to 3/4"で予熱が重要な理由

Thin material sheds heat quickly, allowing hydrogen to escape the HAZ readily — lowest preheat tier in Table 5.11.

A36に32°Fが適用される理由

最低予熱32°F(0°C)は、氷点以上の条件では積極的な予熱が不要であることを意味します。表5.11 カテゴリーAは、A36を非低水素SMAWで溶接する場合、この板厚では延性が十分で炭素当量が低いため水素割れのリスクが最小限であるとして、周囲温度を最低値として設定しています。脚注(a)により、32°F未満で作業する場合は、継手を少なくとも70°F(20°C)まで予熱し、溶接中も維持すること。

SMAW (non-low-hydrogen)とup to 3/4"における他の鋼材

鋼材カテゴリー予熱
A53 Gr.BA32°F (0°C)
A106 Gr.BA32°F (0°C)

別の組み合わせを試す

インタラクティブ予熱計算機を使用して、D1.1:2025 表5.11のあらゆる鋼材・プロセス・板厚の組み合わせを検索できます。

up to 3/4"でSMAWを使用したA36の最小予熱温度は?
A36をSMAW (non-low-hydrogen)でup to 3/4"の板厚で溶接する場合、最低予熱温度はAWS D1.1:2025 表5.11、カテゴリーAに基づき32°F(0°C)です。これはパス間温度の最低値でもあり、パス間でも継手が32°F以下に冷却されてはなりません。
A36とSMAWに適用される表5.11のカテゴリーは?
SMAW (non-low-hydrogen)で溶接されたA36は、AWS D1.1:2025 表5.11のカテゴリーAに該当します。非低水素SMAWプロセス。up to 3/4"板厚では、このカテゴリーは最低予熱32°F(0°C)を要求します。
up to 3/4"でA36に予熱は必要?
SMAW (non-low-hydrogen)でのup to 3/4"板厚では、最低予熱は32°F(0°C)— 実質的に氷点以上の周囲温度です。母材が32°F未満でない限り、積極的な予熱は不要です。表5.11 脚注(a)により、氷点下で作業する場合は少なくとも70°F(20°C)まで予熱し、溶接中も維持すること。

D1.1:2025参考データ。AWSとの提携なし。