M270M Gr.345S予熱 — H8、Mid HI、20–40 mm: 150°F
AASHTO/AWS D1.5:2025(橋梁溶接規格)に基づく、20–40 mm (3/4–1½ in)板厚、水素指定H8でのにおけるM270M Gr.345S / M270 Gr.50Sの破壊臨界予熱要件。
AWS D1.5:2025に基づく — すべての値は条項に追跡可能。
M270M Gr.345S / M270 Gr.50S
AASHTO M270M Gr.345S (M270 Gr.50S) is the structural shape variant of Gr.345, intended for rolled W-shapes and channels used in bridge framing. The "S" suffix indicates the shape-specific chemistry and mechanical property requirements. Used in cross-frame angles, diaphragm members, and built-up sections where rolled shapes are specified rather than plate. Preheat requirements match Gr.345 — Table 6.3 Group 1 for NFC, Tables 12.4/12.5 for FC applications.
M270M Gr.345S / M270 Gr.50SのFC予熱を理解する
Shape-grade 345 MPa (50 ksi) steel for rolled bridge members. Under D1.5 fracture-critical requirements (Clause 12), the combination of H8 hydrogen designation and this heat input band requires 150°F minimum preheat at 20–40 mm (3/4–1½ in). Lower hydrogen levels (H4 < H8 < H16) allow lower preheat because less hydrogen enters the weld deposit. Similarly, higher heat input reduces preheat requirements because slower cooling rates give hydrogen more time to diffuse out.
M270M Gr.345S / M270 Gr.50Sの使用箇所
Used as rolled W-shapes and channels in bridge cross-frames, diaphragm members, and built-up sections. The "S" shape designation indicates procurement under AASHTO M270 with shape-specific chemistry and mandatory CVN testing. Common applications include WT sections for cross-frame members, MC channels for diaphragms, and W-shapes for floor beams on shorter spans. Weld details are primarily fillet welds at gusset connections and clip angles.
M270M Gr.345S / M270 Gr.50SにおけるH8水素管理
For Gr.345S (50S) rolled shapes, H8 is adequate for most connection details where the weld length is short and access allows proper preheat application. Cross-frame gusset connections rarely justify the cost premium of H4 consumables when H8 meets the FC preheat budget.
20–40 mm (3/4–1½ in)で予熱が重要な理由
Material from 20 to 40 mm (3/4 to 1-1/2 in) includes many girder web plates, splice plates, and bearing stiffener plates. Preheat increases to 20°C (70°F) for Group 1 and 50°C (125°F) for Group 2 under Table 6.3. The thicker section slows hydrogen diffusion, requiring higher preheat to maintain safe cooling rates.
20–40 mm (3/4–1½ in)でのM270M Gr.345S / M270 Gr.50S
At 20–40 mm flange thickness, Gr.345S (50S) W-shapes serve as floor beams on shorter spans and as bracing members in steel box girders. Connection details include moment connections to girder webs requiring CJP flange welds with backing bars. Preheat is applied to the thicker element at the connection — when a 25 mm shape connects to a 50 mm plate, preheat must meet the requirement for the 50 mm thickness tier.
H8 2.0–2.8 kJ/mm · 20–40 mm (3/4–1½ in)における他の橋梁鋼材
| 鋼材 | 表 | 予熱 |
|---|---|---|
| M270M Gr.250 / M270 Gr.36 | A | 150°F (70°C) |
| M270M Gr.345W / M270 Gr.50W | B | 200°F (90°C) |
| M270M HPS345W / M270 HPS50W | B | 200°F (90°C) |
| M270M HPS485W / M270 HPS70W | B | 200°F (90°C) |
H8 2.0–2.8 kJ/mmでのM270M Gr.345S / M270 Gr.50S
別の組み合わせを試す
D1.5橋梁予熱計算機を使用して、AASHTO M270鋼材の水素レベルと入熱の任意の組み合わせを検索できます。構造用鋼にはD1.1予熱計算機もご覧ください。
関連ガイド
D1.5:2025参考データ。AWSおよびAASHTOとの提携なし。