AWS D1.1:2025 · तालिका 5.11 · श्रेणी A

A516 Gr.55/60 SMAW (non-low-hydrogen) के लिए पूर्वतापन — 1-1/2" to 2-1/2"

A516 Gr.55/60 को SMAW (non-low-hydrogen) से 1-1/2" to 2-1/2" मोटाई पर वेल्ड करने के लिए न्यूनतम पूर्वतापन और अंतरपास तापमान, AWS D1.1:2025 तालिका 5.11 के अनुसार।

AWS D1.1:2025 तालिका 5.11 पर आधारित — प्रत्येक मान खंड तक ट्रेस किया गया।

न्यूनतम पूर्वतापन और अंतरपास तापमान
225°F / 110°C
श्रेणी A
गैर-कम-हाइड्रोजन SMAW प्रक्रिया
AWS D1.1:2025 तालिका 5.11, §5.7
संदर्भ उपकरण। परियोजना-लागू संस्करण और इंजीनियर-अनुमोदित WPS के विरुद्ध सत्यापित करें।

SMAW (Non-Low-Hydrogen)

Non-low-hydrogen SMAW (E6010/E6011) uses cellulosic electrodes with higher hydrogen potential, assigned to Category A in Table 5.11.

For pressure vessel plate, non-low-hydrogen SMAW is typically limited to non-pressure attachments and temporary fit-up clips. Code requirements per ASME Section VIII often mandate low-hydrogen processes for pressure-retaining welds. Any E6010 tack welds on pressure boundaries must be completely removed before final low-hydrogen welding.

SMAW Tips for Pressure Vessel and Low-Temperature Steels

For A516 Grades 55/60 pressure vessel plate (30–32 ksi yield, Category A), non-LH SMAW is prequalified for non-pressure attachments and structural members. However, ASME Code construction for pressure-retaining welds on A516 requires low-hydrogen processes per ASME Section II and III requirements — E6010 is generally NOT acceptable for pressure-retaining vessel welds under the boiler and pressure vessel codes.

Typical values for reference — always verify against your approved WPS and electrode manufacturer data.

Why SMAW (non-low-hydrogen) for A516 Gr.55/60 at 1-1/2" to 2-1/2"

Why SMAW (non-low-hydrogen) for A516 Gr.55/60 at 1-1/2" to 2-1/2"? SMAW (non-low-hydrogen) delivers 3-5 lb/hr deposition — compared to SAW at 15-40 lb/hr. Position capability: all positions. Suitability: field and shop.

A516 Gr.55/60

ASTM A516 Grades 55 and 60 are carbon steel plates designed for moderate and lower temperature pressure vessel service. Grade 55 (55 ksi tensile, 30 ksi yield) and Grade 60 (60 ksi tensile, 32 ksi yield) are widely used in storage tanks, heat exchangers, and process drums. Chemistry limits (0.24% max carbon for Gr.55, 0.27% max carbon for Gr.60 on thicker plate) and typical carbon equivalent of 0.38-0.44 qualify them for both Category A (non-low-hydrogen) and Category B preheat in Table 5.11. A516 is produced in plate thicknesses from 1/4" through 12". Grades 55 and 60 may be ordered as-rolled, normalized, or stress-relieved depending on the ASME Code requirements for the specific vessel design temperature and thickness.

A516 Gr.55/60 के लिए SMAW के साथ यह पूर्वतापन क्यों

Pressure vessel plate for storage tanks and heat exchangers at moderate strength. At this thickness, SMAW with non-low-hydrogen electrodes places the joint in Category A of Table 5.11. The minimum preheat of 225°F compensates for the higher diffusible hydrogen from cellulosic electrode coatings. The thicker the material, the longer hydrogen takes to escape the heat-affected zone, which is why preheat rises with thickness even for this common grade.

A516 Gr.55/60 के सामान्य अनुप्रयोग

Specified for atmospheric storage tank shells per API 650, heat exchanger tube sheets, air receiver vessels, condensate drums, deaerator shells, and low-pressure separator vessels. A516 Gr.60 is the workhorse for ASME VIII Division 1 vessels under 650°F design temperature. Shell-to-head circumferential seams and nozzle reinforcement pads are the primary weld details. Plate thicknesses for API 650 tank shells typically range from 5/16" at the top course to 1" or more at the bottom course depending on tank diameter and liquid specific gravity. Vertical seam welds carry the full hydrostatic head and require complete joint penetration with radiographic examination. Tank diameters range from 15 feet for small day tanks to over 300 feet for crude oil terminal storage. Shop-welded vessel shells are rolled from flat plate with longitudinal seams welded first, then circumferential seams joining shell courses together on the vessel rotator.

1-1/2" to 2-1/2" पर पूर्वतापन क्यों महत्वपूर्ण है

Heavy plate with significant restraint and thermal mass — preheat is critical to maintain slow cooling for hydrogen escape.

1-1/2" to 2-1/2" पर SMAW (non-low-hydrogen) के साथ अन्य स्टील

स्टीलश्रेणीपूर्वतापन
A36A225°F (110°C)
A53 Gr.BA225°F (110°C)

A516 Gr.55/60 SMAW (non-low-hydrogen) के साथ

विभिन्न संयोजन आज़माएँ

D1.1:2025 तालिका 5.11 से किसी भी स्टील, प्रक्रिया और मोटाई संयोजन को देखने के लिए इंटरैक्टिव पूर्वतापन कैलकुलेटर का उपयोग करें।

1-1/2" to 2-1/2" पर SMAW के साथ A516 Gr.55/60 के लिए न्यूनतम पूर्वतापन क्या है?
1-1/2" to 2-1/2" पर SMAW का उपयोग करके A516 Gr.55/60 की वेल्डिंग करते समय, न्यूनतम पूर्वतापन तापमान 225°F (110°C) है, AWS D1.1:2025 तालिका 5.11, श्रेणी A के अनुसार। SMAW इस संयोजन को श्रेणी A में रखता है। यह न्यूनतम अंतरपास तापमान भी है — जोड़ पास के बीच 225°F से नीचे ठंडा नहीं होना चाहिए।
SMAW के साथ A516 Gr.55/60 पर कौन सी तालिका 5.11 श्रेणी लागू होती है?
A516 Gr.55/60 पर SMAW का उपयोग करते समय, संयोजन AWS D1.1:2025 तालिका 5.11 में श्रेणी A के अंतर्गत आता है। गैर-कम-हाइड्रोजन SMAW प्रक्रिया। 1-1/2" to 2-1/2" मोटाई पर, SMAW के साथ श्रेणी A के लिए न्यूनतम 225°F (110°C) पूर्वतापन आवश्यक है।
1-1/2" to 2-1/2" पर A516 Gr.55/60 के लिए पूर्वतापन 225°F क्यों है?
SMAW का उपयोग करते समय 1-1/2" to 2-1/2" पर A516 Gr.55/60 के लिए 225°F पूर्वतापन स्टील की कठोरणीयता और इस मोटाई पर बढ़े हुए प्रतिबंध के संयोजन को दर्शाता है। SMAW नियंत्रित हाइड्रोजन स्तर प्रदान करता है, लेकिन इस मोटाई पर पूर्वतापन को ताप-प्रभावित क्षेत्र में शीतलन दर धीमी करनी चाहिए, जिससे विसरणशील हाइड्रोजन को स्टील के दरार-संवेदनशील सूक्ष्म संरचना में बदलने से पहले बाहर निकलने का अधिक समय मिले।

D1.1:2025 संदर्भ डेटा। AWS से संबद्ध नहीं।