AWS ER70S-6 · WFS LookupDrahtvorschub-Rechner
Wählen Sie den Drahtdurchmesser und geben Sie die Stromstärke ein, um die veröffentlichten Verfahrenszeilen von Lincoln SuperArc L-56 abzufragen. Zurück kommen Drahtvorschub (ipm), Spannung und Abschmelzleistung als Bereichsbänder gegenüber der Herstellerhülle. Umfang: Massivdraht ER70S-6 aus unlegiertem Stahl; nur veröffentlichte Gas- und Lichtbogenarten; keine Interpolation zwischen Lincoln-Zeilen.
Lincoln SuperArc L-56 (AWS A5.18 / ER70S-6) published operating-procedure rows for Kohlenstoffstahl Massivdraht only. Short-Circuit Transfer assumes 100% CO2 shielding; Sprühlichtbogen assumes 90% Ar / 10% CO2 shielding. Polarität is DC Elektrode positive for all rows. Other gas blends, transfer modes, wire chemistries (stainless, aluminum, low-alloy, metal-cored, flux-cored), and base-metal alloys require their own vendor procedure tables.
Still have questions? Answers from 80 welding standards — with the clause number.
So funktioniert der eingeklammerte Bereich
Die Tabelle Typical Operating Procedures von Lincoln SuperArc L-56 veröffentlicht drei Arbeitspunkte je Drahtdurchmesser und Lichtbogenart. Jeder Punkt ist ein vollständiges Tupel: Drahtvorschub (ipm), Spannung (V), Strom (A) und Abschmelzleistung (lb/hr). Liegt die Stromstärke zwischen zwei veröffentlichten Zeilen, klammert der Rechner die Eingabe und zeigt den Vorschubbereich zwischen diesen Zeilen. Trifft sie eine Zeile genau, schrumpft der Bereich auf diese Zeile.
Die Verfahren in diesen Bereichen gelten für den Kurzlichtbogen mit 100 % CO2. Bei 75 % Argon und 25 % CO2 im Kurzlichtbogen die Spannung um 1 bis 2 Volt senken.
Lincoln SuperArc L-56 Product Technical Data Sheet, Typical Operating Procedures Tabelle footnote (6)
Dieser Rechner extrapoliert nicht über die von Lincoln veröffentlichte Hülle hinaus. Liegt die Stromstärke unter dem kleinsten veröffentlichten Wert für den gewählten Draht und die Lichtbogenart, zeigt das Ergebnis eine Markierung außerhalb des Bereichs und rät zu einem dünneren Draht oder einer anderen Lichtbogenart. Liegt sie über dem größten veröffentlichten Wert, rät es zu einem größeren Durchmesser. Außerhalb der veröffentlichten Hülle zu arbeiten heißt, ohne vom Hersteller geprüfte Verfahrensdaten zu schweißen; fragen Sie die WPS der Werkstatt oder den technischen Support des Drahtherstellers.
Quellenangabe
This calculator's encoded values trace directly to the Lincoln SuperArc L-56 Product Technical Data Sheet, an AWS A5.18 / ER70S-6 carbon-steel solid wire. The Typical Operating Procedures table publishes 21 operating-point rows across 7 wire-diameter and transfer-mode combinations (0.030 SC, 0.035 SC, 0.035 SP, 0.045 SC, 0.045 SP, 0.052 SP, 1/16-in SP). All rows are encoded verbatim with per-row anti-fact tests pinning each value.
Document fingerprint — Published 2012-02-06; SHA256 b45ea7b8c8d1b59152a3907f8f91b29c53c29fdcef09ab931133a4dfb0d683a1; 247,322 bytes. Independently verified via two byte-identical Startseite Depot CDN mirrors of the same Lincoln document, confirming the procedure table has not been silently mutated since publication. A separate Lincoln content-delivery copy returned the same procedure-table values in a different document layout.
Wire conformance — Lincoln SuperArc L-56 conforms to AWS A5.18 and is classified as ER70S-6. AWS A5.18 specifies the chemistry and Minimum tensile / yield / elongation / impact values for the classification; vendor procedure tables like Lincoln's go beyond the Norm to publish typical operating points for shop use. Other ER70S-6 wires from other manufacturers will have similar but not identical operating envelopes. This calculator encodes Lincoln's specific published table; substituting a different ER70S-6 wire requires that manufacturer's own procedure data.
Drei Referenzabfragen
Überprüfen your inputs against these reference lookups. All three use the encoded Lincoln SuperArc L-56 Typical Operating Procedures rows.
Example 1 — 0.035 wire, 175 A. Matches Lincoln's published Short-Circuit Transfer row for 0.035 in (0.9 mm) at 250 ipm / 22 V / 175 A / 4.0 lb/hr exactly. In-range badge: yes (Lincoln SC envelope for 0.035 wire is 80-175 A). The result card shows all three SC rows for 0.035 wire plus all three Spray Transfer rows (375-600 ipm / 195-275 A) so the user can see the full operating window for this wire diameter.
Example 2 — 0.045 wire, 310 A. Falls between Lincoln's published Spray Transfer rows for 0.045 in (1.1 mm) at 285 A (350 ipm) and 335 A (475 ipm). In-range badge: yes (Lincoln SP envelope for 0.045 wire is 285-340 A). WFS bracket: 350-475 ipm. The result card shows all three SP rows plus, for context, the three SC rows for the same wire (145-200 A, 125-200 ipm) so the user sees both transfer modes.
Example 3 — 0.062 wire, 500 A. Above Lincoln's published Spray Transfer envelope for 1/16 in (1.6 mm) wire, which caps at 430 A (290 ipm). Out-of-range badge with guidance to verify against shop WPS or contact Lincoln Applications Engineering. The result card still shows all three published rows so the user sees how far above the envelope they are.
Häufige Fragen
Weitere Schweißwerkzeuge
Lincoln SuperArc L-56 · AWS A5.18 / ER70S-6 · TDS published 2012-02-06